§ 415.225 - New source performance standards (NSPS).

(a) Any new source subject to this subpart producing titanium dioxide by the sulfate process must achieve the following new source performance standards (NSPS):

Subpart V—Titanium Dioxide-Sulfate Process

Pollutant or pollutant property NSPS effluent limitations Maximum for any 1 day Average of daily values for 30 consecutive days Kg/kkg (or pounds per 1,000 lb) of product TSS11030 Iron (T)4.11.2 Chromium (T)0.270.14 Nickel (T)0.180.095 pH( 1)( 1)

1 Within the range 6.0 to 9.0.

(b) Any new source subject to this subpart producing titanium dioxide by the chloride process must achieve the following new source performance standards (NSPS):

Subpart V—Titanium Dioxide-Chloride Process

Pollutant or pollutant property NSPS effluent limitations Maximum for any 1 day Average of daily values for 30 consecutive days Kg/kkg (or pounds per 1,000 lb) of product TSS144.0 Iron (T)0.520.16 Chromium (T)0.0230.012 ph( 1)( 1)

1 Within the range 6.0 to 9.0.

(c) Any new source subject to this subpart producing titanium dioxide by the simultaneous beneficiation-chlorination (chloride-ilmenite) process must achieve the following new source performance standards (NSPS):

Subpart V—Titanium Dioxide-Chloride-Ilmenite Process

Pollutant or pollutant property NSPS effluent limitations Maximum for any 1 day Average of daily values for 30 consecutive days Kg/kkg (or pounds per 1,000 lb) of product TSS8.42.4 Iron (T)0.320.096 Chromium (T)0.0140.0072 Nickel (T)0.0200.010 pH( 1)( 1)